The release curve and the depot behind it

A release curve shows how much drug has left a depot, and each feature of it (burst, lag, second phase, plateau) has more than one physical cause. Depot mass on the same timeline narrows the list. In extruded PLGA implants, the final rapid release coincided with wet mass starting to climb, in all three setups tested, while dry mass held about constant through the first week.

What does a release curve measure?

A release curve measures how much drug reached the medium and when. It can’t tell you which of several processes moved it there. Fredenberg and colleagues’ review of PLGA systems says release is complex enough to make results hard to generalize and release hard to predict. Bassand and colleagues list water entering, degradation, drug dissolving and diffusing, an acidic pocket inside the depot, pores closing, swelling and the depot breaking apart.

Several of those leave a trace on a balance. Solvent leaving and polymer eroding both take mass out, while water entering puts it in. A mass curve on the same timeline rules some readings in and others out. In vitro release testing covers the release side, and polymer degradation testing the carrier side.

Which depot event sits behind each part of the curve?

Each row lists candidates, and the mass columns say which ones a balance can separate. The phase names follow Bassand and colleagues, who put a typical PLGA burst in the first few hours or 1 to 2 days.

Curve feature What the depot may be doing What wet and dry mass add What mass can’t settle
Burst, first hours to 1 to 2 days Solvent leaving and carrying drug out; drug at or near the surface dissolving A wet mass dip says solvent is leaving faster than water enters. Dry mass falls by the solvent that has left Whether the drug left with the solvent or from the surface
Lag or slow middle Water entering; chains breaking without mass loss; surface pores closing Flat dry mass says little has left, within the balance’s resolution and any residual solvent. Slowly rising wet mass shows water uptake Whether chains are breaking. That takes molecular weight on separate samples
Second phase Swelling that opens the matrix; erosion beginning A sharp wet mass rise, or a peak, near the upturn points to swelling. Dry mass falling points to erosion How much of the wet mass change is water and how much is polymer, without a dry sample
Plateau below 100% Drug still inside; drug degraded, bound or adsorbed; drug lost to sampling Mass still high says the depot may hold the drug. Mass near zero says the drug went somewhere else Which of the other routes took the drug. That takes a recovery check

A green cumulative release curve and a blue depot wet mass curve on one time axis, divided into burst, lag, second phase and plateau, with the wet mass curve holding about level during the burst, rising through the lag, climbing to a peak during the second phase and falling as the depot erodes

Illustrative schematic. An in situ forming depot with drug release and wet mass on one time axis. Shapes and timings vary by formulation, and the axes carry no values.

What is the depot doing during the burst?

In a solvent-based depot, much of the burst happens while the depot forms. Hopkins and colleagues measured 48% of a mock drug released in the first 24 hours from 52 kDa PLGA implants, against 26% from 15 kDa implants, and tied the burst to solvent leaving while the shell formed. Initial burst release covers the causes in depth.

The balance shows the same event from the depot’s side. Lin and colleagues saw drug-free in situ implants lose weight within the first day. Those implants lost 67% (acid-capped PLGA) and 51% (ester-capped) of their NMP in that day, and water coming in couldn’t make up for it. They reported the dip only for the drug-free implants, and leuprolide slowed early NMP release, so a loaded depot may show a smaller dip or none. Where a dip does appear, solvent is leaving faster than water is entering.

What is happening during a lag?

During a lag, the depot is mostly taking up water and breaking chains, and little is leaving. Zolnik and Burgess saw the burst and lag phases of PLGA microspheres look alike at pH 7.4 and pH 2.4, while the second phase ran much faster in acid. PLGA degradation and release explains why chains shorten before mass moves.

A flat dry mass curve fits a lag, and a flat wet curve can mean the matrix is still holding together. In Lin’s ester-capped implants with leuprolide, release stayed limited from about day 9 to day 36 before a final fast phase, and the implants’ weight and volume held steady to day 30. The authors read the steady weight as incomplete polymer degradation.

A lag doesn’t always follow a burst. Ghassemi and colleagues saw no octreotide release at all for the first 10 to 15 days from commercial PLGA microspheres.

What starts the second phase?

In the studies checked here, the second phase starts near a swelling event, and the authors disagree on what drives it. Bassand and colleagues followed solvent-free, extruded PLGA implants loaded with ibuprofen, in buffer and in two agarose gel setups, tracking release, wet mass, volume, dry mass and molecular weight. In every setup, the swelling onset coincided with the onset of the final rapid release, and the setups ranked the same way for both. Dry mass held about constant for the first week and then fell. They propose swelling as the trigger, as a hypothesis from one drug and one polymer.

For microspheres, Zolnik and Burgess tie post-burst release to falling molecular weight instead.

Two in situ systems put the upturn near the wet mass peak rather than at the swelling onset:

  • Fisher’s scaffolds: in a composite of PLGA, polymer microparticles and 30% hydroxyapatite, clodronate release rose to 3% a day at day 20, which the authors matched to peak swelling of 110% to 120% of wet mass between days 20 and 30. The mass data came from separate samples made with unloaded microparticles.
  • Lin’s acid-capped implants: with leuprolide alone, peak weight and volume came at day 11, the start of the final fast release. With leuprolide and a contrast agent, the final release began around day 9 and volume peaked at day 13. Lin and colleagues tie the weight and volume changes to solvent release, and the final fast phase to polymer degradation.

A sharp rise near the upturn says water is flooding the matrix, and a later fall says material is leaving faster than water enters. Polymer degradation testing shows release picking up before dry mass falls.

Why does a curve plateau below 100%?

Either the drug is still in the depot, or it went somewhere the assay doesn’t count. A mass curve on the same depots can point to the branch: mass still high leaves room for drug inside, and a depot that’s gone rules that out.

Ghassemi’s octreotide microspheres show the second branch, though the authors didn’t weigh them. Release plateaued at 85% of the loading, and they report the microspheres fully degraded by day 95. Of the peptide that came out, 75% was acylated, bonded to the polymer’s breakdown products. By our arithmetic (85% released times 25% native), an assay that counted only native peptide would have shown about 21%. The authors put the missing 15% down to insoluble peptide residue or adsorption to surfaces.

On the first branch, a plateau with the depot’s mass still high can also be a long lag, so check that the run has finished before you call it a plateau. Then extracting the residual drug answers the question. The recovery section of the release testing guide lists the checks for filters, membranes and drug stability.

What if the two curves disagree?

A disagreement rules out any mechanism that would move both curves. These readings are ours rather than a published rule:

  • Release rises, mass holds flat: drug is leaving by diffusion through pores or from the surface, before swelling or erosion. Molecular weight shows whether the matrix is close to giving way.
  • Mass rises, release holds flat: the depot is taking up water and still holding the drug. Check the drug’s solubility in the medium before you read this as a formulation trait.
  • Mass falls, release holds flat: solvent or polymer is leaving without drug. Late in a run, that sends you to the plateau checks above.
  • Both shift together when the setup changes: the timing belongs to the depot.

Check the setup first. Bassand and colleagues asked whether their gel was simply holding drug back from the assay. They measured the drug held in the gel and attribute most of the gap in release to the implant swelling later.

What can’t a mass curve settle?

A wet mass curve sums water, polymer, solvent and drug. It can’t split them. Dry mass splits off the water, and molecular weight shows chain breaking. Both end the run for the depot you sample. Mass loss, molecular weight and erosion covers how to run them.

Pairing also depends on the design. Bassand and Fisher weighed separate sets from the depots they sampled for release, so their comparisons cross sample sets. Lin ran release alongside the weighing and imaging, on implants from the same batch. Match the timepoints too, or the comparison crosses time as well as samples. Depot release methods compared covers how the method itself shifts the curve.

What a GelTech study measures on release and depot behavior

A GelTech study records depot mass and drug release on one timeline. Carousel tracks drained wet mass at every timepoint, to 1 mg, six samples at a time, for weeks to months. Integrated instruments such as UV-Vis, HPLC and LC-MS read the drug in sampled medium. Molecular weight runs in GelTech’s lab on separate samples, for the stretch where chains break before mass moves.

Samples run for weeks to months at the temperature and pH you set: closer to in vivo conditions, and a stronger basis for IVIVC. That describes the test conditions, and an IVIVC still rests on the in vivo data it’s built against.

GelTech doesn’t run animal or clinical studies, or accredited biocompatibility or sterility testing. See drug delivery, how a pilot study works and the study brief checklist.

Sources

Related reading

GelTech services and industries

Questions

Does every PLGA depot release in three phases?

PLGA depots don't always release in three phases. Bassand and colleagues note that mono-, bi- and triphasic profiles all occur: a depot with no drug at its surface shows no burst, and a depot that empties before it swells shows no final rapid phase. Their extruded implants had a non-porous surface and showed no burst at all.

Should release and mass come from the same depots?

Release and mass from the same depots take depot-to-depot variation out of the comparison, which matters most when the two curves turn within a day or two of each other. Only wet mass can be read without ending a depot's run, so a study that also wants dry mass or molecular weight plans extra depots for every timepoint, and those comparisons cross sample sets.

Can a gel around the depot change the release curve?

A gel around a PLGA implant can slow its release, because it holds back swelling. Bassand and colleagues embedded ibuprofen implants in agarose to stand in for tissue. Release took longer in both gel setups than in bulk buffer, and swelling started later in the gels too.

Does a falling molecular weight explain when the second phase starts?

A falling molecular weight shows that chains are breaking, and it didn't time the second phase on its own in one implant study. Bassand and colleagues saw molecular weight fall about equally across three setups over the first 6 days, while swelling and the release upturn came at different times. They read swelling as the trigger, once degradation had weakened the matrix enough.

A row of palm trees against a blue sky

Need a material characterized?

Send your formulation and plan the study with the team.

By sending, you agree to our terms and privacy policy. Please leave out confidential formulation details until an NDA is in place.