Injectable hydrogels for drug delivery
An injectable hydrogel either thins under shear and recovers after the needle, or goes in as a liquid and gels in the body by temperature, ions or a chemical reaction. Each route fails differently. In one study, one PEG-PLGA thermogel shrank by about 25% within 6 hours at 37 °C, measured as the water it expelled, while another didn’t shrink, so test after injection as well as before.
How do injectable hydrogels form?
Injectable hydrogels form by gelling in the body, by flowing under shear and recovering, or, less often, by collapsing for injection and recovering their shape. Li and Mooney describe those three groups: in situ gelling, shear-thinning and macroporous gels. The four routes below fall into the first two.
- Shear-thinning and self-healing: the gel is formed in the syringe. Chen, Burdick and colleagues define shear-thinning as viscosity falling as shear rises, and self-healing as the gel reforming once the load stops.
- Temperature: a thermosensitive solution that’s fluid at room temperature gels near body temperature. Poloxamer 407 and PLGA-PEG-PLGA triblock copolymers are the common examples.
- Ions: a polymer such as alginate gels when divalent cations like calcium bridge its chains. It can go in already gelled, or mixed with a slow calcium source so it sets after injection.
- Chemical crosslinking: two components react after mixing, by Michael addition or click chemistry, and form covalent bonds.
The readouts these gels share with any drug-delivery hydrogel are set out in hydrogel characterization for drug delivery. The injection step adds the tests below.
What should you test before injection?
Before injection, test whether the formulation flows through the needle and gels at the right temperature and speed. Li and Mooney put the gelation window in one sentence: ideal kinetics are “slow enough to prevent needle clotting, but fast enough to prevent dilution of the pre-gel solution by body fluids once in the body”.
- Viscosity and shear thinning: a shear-rate ramp shows how far viscosity falls at injection rates. For a thermogel, the poloxamer review by Marques and colleagues describes flow that’s Newtonian at low temperature and shear-thinning at higher temperature.
- Gelation temperature: Marques and colleagues list tube inversion, a stir bar that stops turning, and the G′ and G″ crossover in oscillatory rheology. They write that visual methods “lack precision and accuracy”, and name rheology and calorimetry as more reliable.
- Concentration: for poloxamer, concentration and gelation temperature “vary inversely”. In Khodaverdi and colleagues’ PLGA-PEG-PLGA, tube inversion, checked by calorimetry, put the transition at about 31.2 °C for a 25% w/v solution and about 34.4 °C for 15%.
- Loaded formulation: measure the transition with the drug in, since a drug can shift it.
- Injection force: measured through the intended needle. The characterization guide summarizes Chen’s published method. Marques and colleagues note that “not many authors” measure the force needed to inject a poloxamer gel.
What should you test after the gel forms?
After gelation, test whether the gel recovers, holds its water, stays intact and releases on schedule. These tests run for weeks, since the depot’s job starts after injection.
- Recovery: Chen and colleagues alternate low strain (0.2%) and high strain (500%) at 10 Hz and watch G′ drop and return. Researchers have explored secondary crosslinking to stabilize physically assembled gels after injection, they note.
- Swelling or shrinkage: a thermogel can contract as it sets. Wei and colleagues held 1 mL of 15% PEG-PLGA solution at 37 °C for 6 hours and measured the water that escaped. One formulation shrank by about 25% and another not at all, and they excluded any above 10%. Citing earlier work, they write that shrinkage “can lead to the expelling of water, resulting in the burst release of proteins dissolved in the water”.
- Degradation or erosion: mass over time in a medium with the ions the body has. For ionic gels, hydrolytic versus enzymatic degradation explains how the medium sets the result, and initial burst release shows what an early mass change does to the first release points.
- Release: read in sampled medium. Depot release methods compared covers how to form the gel in the vessel and which method fits.
The swelling arithmetic sits on the hydrogel swelling ratio page, and reading the moduli beside the mass curve is the subject of hydrogel rheology and swelling.
Which tests fit which gelation route?
Each route has its own failure, so each needs its own emphasis in the test plan. The table draws on Li and Mooney and the papers cited above, and the pairings of route and test are our reading of them.
| Gelation route | Example systems | What to test | Typical failure |
|---|---|---|---|
| Shear-thinning, self-healing | Gels with reversible crosslinks, such as the hyaluronic acid gels in Chen’s protocol | Shear-rate ramp, strain sweep, cyclic strain recovery, behavior after extrusion | Slow or partial recovery, and a gel that breaks up after injection |
| Temperature | Poloxamer 407, PLGA-PEG-PLGA | Transition temperature on the loaded gel, shrinkage at 37 °C, erosion, release | Fast erosion with burst (poloxamer), water expelled as the gel shrinks |
| Ions | Alginate with calcium | Gelation rate by calcium source, mass over time in a sodium-containing medium | Uneven gel from fast gelation, crosslinks lost to sodium exchange |
| Chemical crosslinking | Michael addition, click chemistry | Gelation time against the injection window, residual reagents, degradation | Needle clogging if fast, dilution if slow, harmful monomers or catalysts |
What trade-offs come with each route?
Every route buys convenience at the cost of something the test plan has to check, and the sources name four trade-offs.
- Pure poloxamer gels erode fast. Marques and colleagues report fast erosion of pure poloxamer gels in aqueous media, with burst release as a result. Khodaverdi’s PLGA-PEG-PLGA gel released vitamin B12 at a near-constant rate for 25 days in vitro, while naltrexone in the same gel followed diffusion kinetics, with a larger burst, for about 17 days.
- Ionic gels trade control for speed. Lee and Mooney write that calcium chloride gives “rapid and poorly controlled gelation”, while calcium sulfate or carbonate slow it and widen the working time, and slower gelation gives a more uniform gel. They put alginate gels’ pores at about 5 nm, which lets small molecules diffuse out fast.
- Chemical gels trade safety margin for strength. Covalent bonds hold longer, but Li and Mooney warn that some pre-gel solutions need “monomers or catalysts that are harmful to cells and tissues”. They put click gelation at a few minutes to an hour, tunable.
- Shear-thinning gels skip the gelation race and depend on recovery instead, which a single modulus measured before injection won’t show.
Which parts of the injection site does a bench test leave out?
A bench test leaves out the tissue the gel lands in, and the release testing guide covers how little liquid a depot first meets there. Dilution by body fluid, which Li and Mooney name as the risk of slow gelation, plays out differently in a vessel of buffer than in tissue.
The tests also judge one formulation at a time. Ranking candidates needs the same conditions for each, as comparing hydrogel formulations explains.
What a GelTech study measures on injectable hydrogels
A GelTech study forms the gel in medium at the temperature and pH you set, then follows it for weeks to months. Carousel weighs each sample’s drained wet mass to 1 mg at every timepoint, six samples at a time, in a 24 mL sample chamber inside a 50 mL incubation chamber. The curve shows when a gel gained or lost mass; telling shrinkage from erosion takes dry mass too, which the release curve and the depot behind it covers. Carousel’s mass data carries roughly 3x less data variability than manual work.
Integrated instruments add rheometry and UV-Vis, HPLC or LC-MS for drug in sampled medium. Depot mass and drug release sit on one timeline: closer to in vivo conditions, and a stronger basis for IVIVC. A chamber still holds far more fluid than an injection site, and Carousel doesn’t replicate the body. GelTech doesn’t run animal or clinical studies, or accredited biocompatibility or sterility testing. See drug delivery and how a pilot study works.
Sources
- Li J, Mooney DJ. Designing hydrogels for controlled drug delivery. Nat Rev Mater. 2016;1:16071
- Chen MH, Wang LL, Chung JJ, Kim YH, Atluri P, Burdick JA. Methods to assess shear-thinning hydrogels for application as injectable biomaterials. ACS Biomater Sci Eng. 2017;3(12):3146-3160
- Marques AC, Costa PC, Velho S, Amaral MH. Injectable poloxamer hydrogels for local cancer therapy. Gels. 2023;9(7):593
- Khodaverdi E, Tekie FSM, Mohajeri SA, Ganji F, Zohuri G, Hadizadeh F. Preparation and investigation of sustained drug delivery systems using an injectable, thermosensitive, in situ forming hydrogel composed of PLGA-PEG-PLGA. AAPS PharmSciTech. 2012;13(2):590-600
- Lee KY, Mooney DJ. Alginate: properties and biomedical applications. Prog Polym Sci. 2012;37(1):106-126
- Wei PS, Chou PY, Hsu HY, et al. Nonshrinkable thermosensitive hydrogels combined with bispecific anti-PSMA/CD3 T-cell engager for effective against tumors in mice model. Int J Nanomedicine. 2025;20:3083-3111
Related reading
GelTech services and industries
Questions
What gelation temperature should a thermogel target?
A thermogel's gelation temperature should sit above room temperature and near body temperature, but never above 37 °C, Marques and colleagues write. Above room temperature avoids premature gelation that impedes injection, and staying at or under 37 °C lets the gel set once it's in the body.
Does a drug change an injectable hydrogel's gelation temperature?
A drug can shift an injectable hydrogel's gelation temperature, so measure it on the loaded formulation. Khodaverdi and colleagues found that vitamin B12 lowered the transition temperature of their PLGA-PEG-PLGA gel, while naltrexone hydrochloride had no significant effect.
Can a poloxamer gel be made strong enough to last longer?
Poloxamer gels can be strengthened, and Marques and colleagues review several routes: a chain extender, bioadhesive polymers such as N,N,N-trimethyl chitosan, alginate or xanthan gum, or chitosan crosslinked with genipin inside the gel. Each additive changes the formulation, so gelation and erosion need testing again.